Malzeme
Rehberi
Home
> Steel > EN X17CrNi16-2
EN X17CrNi16-2
ISO EN X17CrNi16-2
Steel
Stainless steel
⚖️ Compare This Material
Mechanical Properties
💪 Yield Strength
600
MPa
🔩 Tensile Strength
800
MPa
📐 Young's Modulus
206
GPa
📏 Elongation at Break
14
%
Physical Properties
⚖️ Density
7860
kg/m³
↔️ Poisson's Ratio
0.3
-
💰 Cost Index
3
/ 10
Feature Tags
Marine Applications
Cryogenic (Low Temp)
Corrosion Resistance
Similar Materials
Steel SAE 3140
ANSI Steel SAE 3140
💪 600 MPa
⚖️ 7860 kg/m³
Steel
EN 25CrMo4
ISO EN 25CrMo4
💪 600 MPa
⚖️ 7860 kg/m³
Steel
DIN 25CrMo4
DIN DIN 25CrMo4
💪 600 MPa
⚖️ 7860 kg/m³
Steel
DIN 30CrV9
DIN DIN 30CrV9
💪 600 MPa
⚖️ 7860 kg/m³
Steel
💡 Did You Try This?
A lighter alternative providing the same yield strength:
CSN 422735
CSN CSN 422735
💪 520 MPa
⚖️ 7160 kg/m³