DIN 37Cr4

DIN DIN 37Cr4
heat treated
Steel Heat-treatment steel
⚖️ Compare This Material

Mechanical Properties

💪 Yield Strength 630 MPa
🔩 Tensile Strength 850 MPa
📐 Young's Modulus 206 GPa
📏 Elongation at Break 13 %
💎 Hardness (HV) 270 HV

Physical Properties

⚖️ Density 7860 kg/m³
↔️ Poisson's Ratio 0.3 -
💰 Cost Index 3 / 10

Feature Tags

-

💡 Did You Try This?

A lighter alternative providing the same yield strength:

CSN 422739
CSN CSN 422739
💪 550 MPa ⚖️ 7160 kg/m³