Malzeme
Rehberi
Home
> Copper > High Leaded Tin Bronze C93800
High Leaded Tin Bronze C93800
ANSI High Leaded Tin Bronze C93800
Copper
Genel
⚖️ Compare This Material
Mechanical Properties
💪 Yield Strength
110
MPa
🔩 Tensile Strength
207
MPa
📐 Young's Modulus
120
GPa
📏 Elongation at Break
18
%
Physical Properties
⚖️ Density
8800
kg/m³
↔️ Poisson's Ratio
0.31
-
💰 Cost Index
3
/ 10
Feature Tags
-
Similar Materials
Red brass C83800
ANSI Red brass C83800
💪 110 MPa
⚖️ 8500 kg/m³
Copper
Tin Bronze C90200
ANSI Tin Bronze C90200
💪 110 MPa
⚖️ 8800 kg/m³
Copper
High Leaded Tin Bronze C93400
ANSI High Leaded Tin Bronze C93400
💪 110 MPa
⚖️ 8800 kg/m³
Copper
High Leaded Tin Bronze C93500
ANSI High Leaded Tin Bronze C93500
💪 110 MPa
⚖️ 8800 kg/m³
Copper
💡 Did You Try This?
A lighter alternative providing the same yield strength:
Red brass C83600
ANSI Red brass C83600
💪 117 MPa
⚖️ 8500 kg/m³